Iron-Nickel Alloy 42НХТЮА
- Chemical composition
Domestic analoguesAl Aluminum 0.6 — 1.0 Fe Iron Rest Si Silicon 0.4 — 0.7 Mn Manganese 0.3 — 0.6 Ni Nickel 41.5 — 43.5 S Sulfur <0.02 Ti Titanium 2.3 — 2.9 C Carbon <0.05 P Phosphorus <0.02 Cr Chromium 5.0 — 5.6 N41XT
H41XTA
42NHTYU (included in 4 standards)
- Analogs in the USA
- 902
NI-SPAN C-902
5223 D AMS
5225 D AMS
5221 D AMS
5223 E AMS
5221 AMS
5223 AMS
5225 AMS
NI-SPAN alloy C-902 Special Metals
N09902 UNS
K70640 UNS
for hair spirals of clockwork. Technical requirements: GOST 10994−74
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | With preset elastic properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 45.61–49.9 | 0.4–0.7 | 0.3–0.6 | 5–5.6 | 2.3–2.9 | 41.5–43.5 | 0.6–1 | < 0.02 | < 0.05 | < 0.02 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$E\cdot 10^{9}$$, $$MPa$$ | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
|---|---|---|
| 20 | 179 | 9 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|
| 1300–1400 | 5 | Tempering 910 ° C, 700 ° C Aging | |||||
| Wire | GOST 10994-74 | 1080–1375 |
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$E\cdot 10^{9}$$ | $$MPa$$ | Elastic modulus |
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |