45H25N35BSL
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 4112-161-00220302-2011 |
57.98–38.15 |
1.2–1.6 |
1–1.51 |
24–27 |
< 0.2 |
34–36 |
< 0.03 |
0.35–0.45 |
< 0.03 |
1.3–1.7 |
< 0.5 |
Information on suppliers
Analogues
| Germany |
European Union |
USA |
| F 1.4852 |
GX40NiCrSiNb35-26 |
Thermax 533 |
Standards