45H28N49V5S
Used for the manufacture of pipes tsentrobezhnolityh for the manufacture of the coils of the tubular furnace installations production of ammonia, hydrogen, ethylene, carbon disulphide, etc., operating in the temperature range 760−1060 °C and a pressure of 3.92 MPa (40 kgf/cm2); tsentrobezhnolityh pipes used as components in equipment for metallurgical, engineering, glass, ceramic, mining and processing petrochemical industry and is intended for the manufacture of blanks and parts used in the composition of the products of aviation and the nuclear industry.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Ni, % | V, % | Pb, % | As, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 1333-047-00220302-02 | 9.93–93.589 | 1–1.5 | < 0.01 | 0.5–1.5 | 26.5–29.5 | 0.0005–0.1 | < 0.2 | < 0.01 | 47.5–50.5 | 0.0005–0.2 | < 0.01 | < 0.01 | < 0.03 | 0.41–0.47 | < 0.03 | < 0.5 | 4.5–5.5 |
Information on suppliers
Mechanical properties at 20 °C
Analogues
| Germany | European Union | USA |
|---|---|---|
| F 2.4879 | G-NiCr28W EN 10295:2002 | Thermax 70 |
Standards
| Standard | Description |
|---|---|
| TU 1333-047-00220302-02 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| V | % | Vanadium |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| δ | % | Elongation after rupture |
| $$\sigma_{0.2}$$ | $$MPa$$ | Tensile stress required to produce a total elongation of 0.2% |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |