45H28N49V5SL
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| TU 4112-161-00220302-2011 |
10.47–93.59 |
1–1.5 |
0.5–1.5 |
26.5–29.5 |
47.5–50.5 |
< 0.03 |
0.41–0.47 |
< 0.03 |
< 0.5 |
4.5–5.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
Cp, Дж/кг·К |
| 20 |
55.4–75.5 |
8000 |
456 |
Casting and technological parameters
| melting point, °C |
| 1370–1400 |
Analogues
| Germany |
European Union |
USA |
| F 2.4879 |
G-NiCr28W EN 10295:2002 |
Thermax 70 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| W |
% |
Tungsten |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| Cp |
Дж/кг·К |
Specific heat of material |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |