48KHVN
for implantable components in surgery (brackets, frames, implants, etc.).
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ni, % | P, % | C, % | S, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST Р 51397 - 99 | < 3 | < 1 | < 2 | 45.82–58 | 19–21 | 9–11 | < 0.015 | < 0.15 | < 0.015 | 14–16 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\sigma_{Y}$$, $$MPa$$ | d5, % | Treatment |
|---|---|---|---|---|---|---|---|---|
| Wire heat treatment. | GOST 51397-99 | 860 | 310 | 10 | ||||
| The wire is half-worked. | GOST 51397-99 | 1370 | 5 |
Analogues
| Germany | USA |
|---|---|
| ALACRITE X.S.H | Udimet L-605 |
Standards
| Standard | Description |
|---|---|
| GOST Р 51397 - 99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| d5 | % | Elongation at break |
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |