49K2FN-VI (Aeralloy 91)
Alloys with high magnetic saturation induction.
It is used for the manufacture of cutting plates rotors solid configuration of small electric machines (allows you to increase the sensitivity and speed).
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-4341-87 | 98.1–98.4 | < 0.3 | < 0.5 | 48–49.5 | 0.03–0.08 | 0.3–1 | 1.6–1.9 | < 0.02 | < 0.03 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-1-4341-87 | TU 14-1-4341-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |