50KF
Primary application. In the form of forgings and rods — for the manufacture of cores of solenoids, pole pieces, equipment magnetic circuits, operating in constant fields. From tapes and strips make packages of ultrasonic transducers, telephone membranes and other magnetic circuits.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| 47–98.7 | < 0.3 | < 0.3 | 48–50 | < 0.5 | 1.3–1.8 | < 0.025 | < 0.05 | < 0.025 |
Information on suppliers
Analogues
| USA |
|---|
| SPEC MIL-A-47182 |