50H-VI
Forgings made of steel and alloys for machine parts.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ni, % |
P, % |
C, % |
S, % |
| TU 14-1-1530-75 |
48.84–99.98 |
< 0.1 |
< 0.5 |
49–50.5 |
0.02–0.035 |
< 0.02 |
< 0.005 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
Cp, Дж/кг·К |
| 20 |
55.4–75.5 |
8000 |
> 456 |
Casting and technological parameters
| melting point, °C |
| 1370–1400 |
Analogues
| Germany |
USA |
| Ni 52 SEW 385 |
Alloy No. 52 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| Cp |
Дж/кг·К |
Specific heat of material |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |