50N3HYU (EP967)
Used for the manufacture of parts, combined with thermal expansion coefficient with silicon.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-3904-84 | < 47.1 | < 0.3 | < 0.4 | 3–3.7 | 49.5–51 | 0.4–0.7 | < 0.02 | < 0.03 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-1-3904-84 | TU 14-1-3904-84 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |