50U0.5 (2)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Ferroalloys | Ferroalloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | V, % | Al, % | As, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-115-43-97 | 32.67–96 | < 2 | < 4 | < 0.4 | 48–60 | < 0.3 | < 0.01 | < 0.1 | < 0.5 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-115-43-97 | TU 14-115-43-97 |