52KFB (52K12F)
Alloy with magnetic energy (16−24)·103 TA/m.
Depending on the content of vanadium and the temperature property can be obtained the desired ratio of the coercive force and residual induction in the range (4,8−32)·103 A/m and 1.2 to 0.65 T. the Alloy becomes magnetic properties Locle cold deformation of 70−90% and subsequent tempering.
Alloy anisotropic.
Used for the production of small permanent magnets.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Magnetic Hard Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | > 36 | < 0.5 | < 0.5 | 52–54 | < 0.5 | < 0.7 | 11.6–12.5 | < 0.025 | < 0.12 | < 0.02 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |