52N-VI
Alloy with an average value of TECL.
It is used to connect with soft glass; TKLR * 1,000,000 in the temperature range from -70 to +550 ºC no more than 11−11.4 [1 / ºC]; high permeability alloy with saturation induction 1.5 T
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precision alloys |
With given TCLE |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Pb, % |
P, % |
C, % |
S, % |
O, % |
N, % |
H, % |
| GOST 10994-74 |
46.42–48.5 |
< 0.2 |
< 0.4 |
< 0.2 |
< 0.2 |
51.5–52.5 |
< 0.015 |
< 0.015 |
< 0.03 |
< 0.015 |
< 0.008 |
< 0.01 |
< 0.001 |
Note: VI - vacuum induction remelting
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
1.6 |
8200 |
420 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
|
|
|
|
|
450–550 |
|
Casting and technological parameters
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| O |
% |
Oxygen |
| N |
% |
Nitrogen |
| H |
% |
Hydrogen |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |