5KD
Casting methods:
Z — sand casting
B — Lost wax casting
K — chill casting
D — injection molding
Mark designation:
h — clean
bees — high purity
och — high purity
l — casting alloys
c — selective
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Zr, % | Al, % | Cd, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.15 | < 0.2 | < 0.02 | < 0.05 | 0.35–0.8 | 0.15–0.35 | 4.5–5.1 | < 0.1 | < 0.02 | < 0.15 | 92.21–94.93 | 0.07–0.25 | < 0.6 |
Information on suppliers
Analogues
| Russia |
|---|
| АМ4,5Кд ГОСТ 1583-93 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Cd | % | Cadmium |