5VB
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Titanium, titanium alloys | Wrought Titanium Alloys |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Ti, % | V, % | Zr, % | Al, % | C, % | O, % | Mo, % | N, % | H, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 19807-91 | < 0.25 | < 0.12 | < 0.003 | 88.711–93.54 | 1–1.9 | < 0.1 | 4.7–6.3 | 0.06–0.14 | < 0.13 | 0.7–2 | < 0.04 | < 0.006 | < 0.3 |
Note: Zirconium content in total with other impurities <0.3
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 19807-91 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Ti | % | Titan |
| V | % | Vanadium |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| C | % | Carbon |
| O | % | Oxygen |
| Mo | % | Molybdenum |
| N | % | Nitrogen |
| H | % | Hydrogen |