67N26M
Used for the production of hot-rolled bars (10−25 mm) and forged rods (26−100 mm) and micron-sized wire (0,03−0,2 mm), used for the manufacture of parts of vacuum devices and for welding of parts made of alloys nikolkaiyevich Н70М27 (ЭП495) and Н70М27Ф (ЭП490).
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-1-1144-74 | > 2 | < 0.25 | < 0.5 | 66–69 | < 0.02 | < 0.035 | < 0.02 | 25–28 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-1-1144-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |