74NMD
Used for the production of cold-rolled strip used for the manufacture of parts of transformers, chokes and relays, working in weak magnetic fields, screens.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Soft Magnetic Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| TU 14-1-231-72 | 9.03–14.95 | 0.15–0.3 | 0.8–1.1 | 7.5–9.5 | 73–76 | < 0.02 | < 0.03 | < 0.02 | 3.6–4 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-1-231-72 | TU 14-1-231-72 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |