75N34H8G3 (EP636)
Used for the production of bimetallic rolled sheet U8/75N34H8G3 for the manufacture of the tuning fork stabilizers and filters.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-1-2198-77 | 52.045–55.9 | 0.2–0.5 | 2.4–3 | 7.8–8.6 | 33–35 | < 0.03 | 0.7–0.8 | < 0.025 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-1-2198-77 | TU 14-1-2198-77 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |