77NMDP
An alloy with a high rectangularity of the hysteresis loop and a low magnetization reversal coefficient.
For the small band of magnetic cores, switching devices, logic elements, shift registers, the trigger systems.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Soft Magnetic Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10160-75 | 9.74–14.24 | 0.1–0.3 | < 1.4 | 4.8–6 | 75.5–78 | < 0.01 | < 0.03 | < 0.02 | 3.9–4.5 |