80NH15R
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Soft Magnetic Precision Alloys |
Chemical composition
| Standard | B, % | Cr, % | Ni, % | Ba, % | C, % |
|---|---|---|---|---|---|
| 3.5–4.5 | 14–16 | 78.92–82.3 | 0.2–0.5 | < 0.08 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| B | % | Bor |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Ba | % | Barium |
| C | % | Carbon |