80NHS
For magnetic cores.
For cores of small transformers, chokes and relays, operating in weak fields, magnetic shields. In small thicknesses (0.05 to 0.02 mm) — for cores of pulse transformers, magnetic amplifiers and solid-state relays, for cores of magnetic heads.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Soft Magnetic Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 12.33–16.7 | 1.1–1.5 | 0.6–1.1 | 2.6–3 | < 0.15 | < 0.2 | 79–81.5 | < 0.15 | < 0.02 | < 0.03 | < 0.02 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|---|
| 20 | 8500 | 0.62 | |
| 100 | 12.9 |
Mechanical properties at 20 °C
Brinell hardness number
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\sigma_{P}$$ | $$MPa$$ | Proportionality limit |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
| $$\psi$$ | % | Reduction in cross section on fracture |