83NF-W
for small cores of transformers and chokes operating in weak fields; alloy has high permeability in weak fields
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | Soft Magnetic Precision Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | 9.54–13.2 | 0.5–1 | < 0.5 | < 0.5 | 82.5–84.2 | 3.8–4.2 | < 0.03 | < 0.02 | < 0.01 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |