97NL (EI996)
for the live and the power of elastic sensing elements, operating at temperatures up to 300 degrees C
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precision alloys | With preset elastic properties |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mn, % | Cu, % | Ni, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 10994-74 | < 0.5 | < 0.2 | 2.1–2.5 | < 0.3 | < 0.1 | 96.05–97.9 | < 0.3 | < 0.01 | < 0.03 | < 0.01 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | Treatment |
|---|---|---|---|---|---|---|
| GOST 10994-74 | 1570–1865 |
Standards
| Standard | Description |
|---|---|
| GOST 10994-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |