9H4M3F2AGST (EK42)
For processing high-strength and heat-resistant materials.
For the manufacture of tools.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tool steel | High speed tool steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Ca, % | Mn, % | Cr, % | Ti, % | Ni, % | РЗЭ, % | V, % | C, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 14-19-95 - 0 | 86.667–89.59 | 0.5–0.7 | < 0.003 | < 0.08 | 0.55–0.75 | 4–4.5 | 0.15–0.25 | 0.04–0.1 | < 0.08 | 1.6–2.1 | 0.87–0.97 | 2.7–3.2 | < 0.6 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 7830 |
Analogues
| CIS, Russia, Ukraine |
|---|
| ЭК42 |
Standards
| Standard | Description |
|---|---|
| TU 14-19-95 - 0 | |
| TU 14-1-3353-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Ca | % | Calcium |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| РЗЭ | % | Rare earth elements |
| V | % | Vanadium |
| C | % | Carbon |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |