Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Primary aluminum |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
Ga, % |
| GOST 11069-2001 |
< 0.015 |
< 0.015 |
< 0.005 |
< 0.002 |
< 0.002 |
< 0.005 |
< 0.003 |
< 99.97 |
< 0.003 |
Information on suppliers
Analogues
| Germany |
USA |
| EN AW-1098 |
1098 |
Standards