A99KV
For the production of flat ingots for rolling into sheets, strips and other semi-finished products.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Primary aluminum |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|
| GOST 9498-79 | 0.003–0.006 | 0.003–0.006 | < 0.001 | < 0.005 | < 0.002 | 99.98–99.994 |