ASF-2
to work in tandem with heat treated (tempered or normalized) shaft
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Anti-friction cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1585-85 | 90.88–94.52 | 1.4–2.2 | 0.3–1 | 0.2–0.5 | 0.03–0.1 | 0.2–0.5 | 0.2–0.5 | 0.15–0.4 | 3–3.8 | < 0.12 |
Information on suppliers
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 1585-85 | 180–229 |
Limit operating modes
| Standard | Нагрузка, $$\textit{MPa}$$ | Скорость, $$\frac{m}{s}$$ | Нагрузка * Скорость, $$MPa * m/s$$ |
|---|---|---|---|
| GOST 1585-85 | 10 | 0.3 | 2.5 |
| GOST 1585-85 | 0.1 | 3 | 0.3 |
Standards
| Standard | Description |
|---|---|
| GOST 1585-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |