ASF-5
to work in a particularly loaded friction units in tandem with heat treated (tempered or normalized) shaft
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Anti-friction cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| GOST 1585-85 | 78.65–86.1 | 2.5–3.5 | 7.5–12.5 | 0.4–0.8 | < 0.2 | 3.5–4.3 | < 0.05 |
Information on suppliers
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 1585-85 | 180–290 | ||
| GOST 1585-85 | 140–180 |
Limit operating modes
| Standard | Нагрузка, $$\textit{MPa}$$ | Скорость, $$\frac{m}{s}$$ | Нагрузка * Скорость, $$MPa * m/s$$ |
|---|---|---|---|
| GOST 1585-85 | 20 | 1 | 20 |
| GOST 1585-85 | 30 | 0.4 | 12.5 |
Standards
| Standard | Description |
|---|---|
| GOST 1585-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |