ASF-6
for use in friction with temperatures up to 300 deg. paired with the shaft are not subjected to thermal treatment.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Anti-friction cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Pb, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| GOST 1585-85 | 90.48–93.6 | 3–4 | 0.2–0.6 | 0.5–1 | 0.5–1 | 2.2–2.8 | < 0.12 |
Information on suppliers
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 1585-85 | 100–120 |
Limit operating modes
| Standard | Нагрузка, $$\textit{MPa}$$ | Скорость, $$\frac{m}{s}$$ | Нагрузка * Скорость, $$MPa * m/s$$ |
|---|---|---|---|
| GOST 1585-85 | 9 | 4 | 9 |
Standards
| Standard | Description |
|---|---|
| GOST 1585-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Pb | % | Lead |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |