ACHV-1
for use in friction with high peripheral speeds paired with a thermally processed (tempered or normalized) shaft.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Anti-friction cast iron |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1585-85 | 91.59–94.77 | 1.8–2.7 | 0.03–0.08 | 0.6–1.2 | < 0.7 | < 0.2 | 2.8–3.5 | < 0.03 |
Information on suppliers
Brinell hardness number
| Rolling | Standard | Classifiers | Value, HBW |
|---|---|---|---|
| GOST 1585-85 | 210–260 |
Limit operating modes
| Standard | Нагрузка, $$\textit{MPa}$$ | Скорость, $$\frac{m}{s}$$ | Нагрузка * Скорость, $$MPa * m/s$$ |
|---|---|---|---|
| GOST 1585-85 | 1.5 | 10 | 12 |
| GOST 1585-85 | 20 | 1 | 20 |
Standards
| Standard | Description |
|---|---|
| GOST 1585-85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |