AD (1015)
For the manufacture of semi-finished products (sheets, tapes, strips, plates, profiles, panels, rods, tubes, wire, stampings and forgings) by hot or cold deformation, as well as ingots and slabs
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Technical aluminum |
Chemical composition
| Standard | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|
| GOST 4784-97 | < 0.05 | < 0.05 | < 0.05 | < 0.1 | < 99 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 2710 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|
| Trumpet | 60 | 20 | |||||
| Round | GOST 21488-97 | 60 | 25 | ||||
| Tape | annealing | 60 | 20–30 | ||||
| Tape | cold-work | 130–145 | 3–5 | ||||
| Profile | 59 | 20 | |||||
| Sheet | 64–78 | 15–18 |
Analogues
| Germany | USA |
|---|---|
| 3.0185 | 1200 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |