AD0E (1011E)
For the manufacture of semi-finished products (sheets, tapes, strips, plates, profiles, panels, rods, tubes, wire, stampings and forgings) by hot or cold deformation, as well as ingots and slabs
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Technical aluminum |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.4 | < 0.1 | < 0.05 | < 0.01 | < 0.01 | < 0.05 | < 0.05 | < 0.05 | < 99.5 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 2710 |
Analogues
| Germany | USA |
|---|---|
| 3.0255 | AA1050 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |