AD35 (1350)
For the manufacture of semifinished products by hot or cold deformation
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Zn, % |
Al, % |
| GOST 4784-97 |
< 0.5 |
0.7–1.3 |
0.6–1.2 |
0.4–1 |
< 0.25 |
< 0.1 |
< 0.1 |
< 0.2 |
95.35–98.3 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
2700 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Trumpet |
GOST 18482-79 |
|
|
|
200 |
100 |
14 |
Quenching and aging |
| Trumpet |
GOST 18482-79 |
|
|
|
270 |
200 |
10 |
Hardening and artificial aging |
| Round |
GOST 21488-97 |
|
|
|
195 |
110 |
12 |
Quenching and aging |
| Round |
GOST 21488-97 |
|
|
|
315 |
245 |
8 |
Hardening and artificial aging |
| Profile |
GOST 8617-81 |
< 100 |
|
|
314 |
245 |
8 |
Hardening and artificial aging |
| Profile |
GOST 8617-81 |
|
|
|
196 |
108 |
12 |
|
Analogues
| Germany |
USA |
| 3.2315 |
A96061 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Al |
% |
Aluminium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |