AD9-1
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | < 1 | 6–8 | < 0.02 | 0.2–0.55 | 0.2–0.6 | < 0.02 | < 1.5 | < 0.5 | < 0.3 | 84.49–93.6 | < 0.02 | < 3 |
Note: Casting methods: H - sand casting; B - lost-wax casting; K - chill casting; D - injection molding. Grade designation: h - pure bees - high purity och - high purity l - cast alloys c - selective
Information on suppliers
Analogues
| Germany | European Union | USA |
|---|---|---|
| AlSi7Mg | EN AB-42000 EN 1676:2010 | SG 70A |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |