ADch
For the manufacture of semi-finished products (sheets, tapes, strips, plates, profiles, panels, rods, tubes, wire, stampings and forgings) by hot or cold deformation, as well as ingots and slabs
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Technical aluminum |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.03 | < 0.03 | < 0.002 | < 0.015 | < 0.005 | < 99.95 |
Information on suppliers
Analogues
| USA |
|---|
| AA1095 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 |