ADS
For the manufacture of semi-finished products (sheets, tapes, strips, plates, profiles, panels, rods, tubes, wire, stampings and forgings) by hot or cold deformation, as well as ingots and slabs
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Technical aluminum |
Chemical composition
| Standard | Fe, % | Si, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|
| GOST 4784-97 | < 0.6 | < 0.5 | < 0.15 | < 0.1 | < 0.1 | < 99 |
Information on suppliers
Mechanical properties at 20 °C
Analogues
| Germany | USA |
|---|---|
| 3.0205 | AA1100 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |