ADS-12
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
| TU 1712-368-110-99 |
< 0.9 |
9.6–12 |
< 0.3 |
< 0.5 |
< 0.15 |
1.5–3.5 |
< 1 |
< 0.5 |
81.05–88.9 |
< 0.1 |
Information on suppliers
Analogues
| Germany |
USA |
| EN AB-46100 DIN EN 1676:2010 |
SG 102A |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mg |
% |
Magnesium |
| Mn |
% |
Manganese |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |