AISI 304L (03H18N11)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant ordinary steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
| ASTM A 240 |
< 67 |
< 0.8 |
< 2 |
17–19 |
10.5–12.5 |
< 0.035 |
< 0.03 |
< 0.02 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Sheet |
|
|
|
|
500 |
40 |
thin |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |