Chemical composition
| Fe | Si | Mn | Ni | Ti | Al | Cu | Pb | Mg | Zn | Sn | Impurities |
| up to 0.6 | 9.5 — 10.5 | until 0.05 | 0.8 — 1.2 | until 0.05 | 84.28 — 86.1 | 2 — 2.5 | until 0.05 | 0.9 — 1.2 | until 0.06 | up to 0.01 | total 0.7 |
For ingots made from primary metals, scrap and non-ferrous metal waste and alloys, and designed for the production of pistons of internal combustion engines. Technical requirements — according to OST 30620−98
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 30620-98 | < 0.6 | 9.5–10.5 | < 0.01 | 0.9–1.2 | < 0.05 | < 0.05 | 2–2.5 | < 0.06 | 0.8–1.2 | 83.78–86.8 | < 0.05 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 30620-98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |