Alloy aluminum AK7M2 (AL14V)
- Chemical composition
Domestic analog — AL14V GOST 2685−75Al Aluminum Rest Fe Iron <1.3 Si Silicon 6.0 — 8.0 Mg Magnesium 0.2 — 0.6 Mn Manganese 0.2 — 0.6 Cu Copper 1.5 — 3.0 Ni Nickel <0.3 Zn Zinc <0.5 Ot Total impurities <2.0
For the manufacture of shaped castings. Technical requirements — according to GOST 1583−93
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 2685-75 | < 1.3 | 6–8 | 0.2–0.6 | 0.2–0.6 | 1.5–3 | < 0.5 | < 0.3 | 85.8–92.1 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| G-AlSi8Cu3 | 328 |
Standards
| Standard | Description |
|---|---|
| GOST 2685-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |