Alloy aluminum AL1
Chemical composition
Analogs in RussiaAl Aluminum Rest Fe Iron <0.8 Si Silicon <0.7 Mg Magnesium 1.25 — 1.75 Cu Copper 3.75 — 4.50 Ni Nickel 1.75 — 2.25 Ti Titanium <0.1 Zn Zinc <0.1 Zr Zirconium <0.1 Ot Total impurities <1.4 AK4 Included in 2 standards
D4 GOST 2171−90
AKD4 GOST 4784−97
1140 GOST 4784−97
AKD4Sh GOST 4784−97
1140Sh GOST 4784−97
- Analogs in the USA
- AA2218 ANSI
B 247 (2218) ASTM B247
A92218 UNS
2218 Included in 5 standards
For the manufacture of shaped castings. Technical requirements GOST 2685−75 Cast aluminum alloys. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|
| GOST 2685-75 | < 0.8 | < 0.7 | 1.25–1.75 | 3.75–4.5 | < 0.1 | 1.75–2.25 | 90.1–93.25 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|---|---|
| 20 | 168 | 2750 | |
| 100 | 22.3 |
Mechanical properties at 20 °C
Brinell hardness number
Casting and technological parameters
| linear shrinkage, % | the temperature of the casting, °C |
|---|---|
| 1.3 | 720 |
Analogues
| Germany | USA |
|---|---|
| GAICu4NiMg | A02420 |
Standards
| Standard | Description |
|---|---|
| GOST 2685-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter | Units of measurement | Description |
|---|---|---|
| linear shrinkage | % | The difference between model dimensions and the model casting |
| the temperature of the casting | °C | The temperature of the molten polymer is extruded from the heating cylinder into the mold |