AL7-4
Engine parts; sealed alloy.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Foundry aluminum alloys |
Chemical composition
| Standard | Si, % | Cu, % | Al, % |
|---|---|---|---|
| GOST 21488-97 | 6.7–7.3 | 3.8–4.2 | 88.5–89.5 |
Information on suppliers
Mechanical properties at 20 °C
Standards
| Standard | Description |
|---|---|
| GOST 21488-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| Cu | % | Copper |
| Al | % | Aluminium |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |