AlMn10 (B)
For alloying and modifying in the production of wrought and cast aluminum alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Aluminium master alloys |
Chemical composition
| Standard | Fe, % | Pb+Cd, % | Si, % | Be, % | Sn, % | Mg, % | Mn, % | Cr, % | Ti, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST Р 53777-2010 | < 0.7 | < 0.0095 | < 0.5 | < 0.0001 | < 0.02 | < 0.5 | 9–11 | < 0.1 | < 0.1 | < 0.2 | < 0.2 | < 0.2 | > 86.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST Р 53777-2010 | GOST R 53777 - 2010 |