Alnisi (UNS)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Ni, % | Al, % |
|---|---|---|---|---|
| > 52.5 | < 1 | < 33 | < 13.5 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ni | % | Nickel |
| Al | % | Aluminium |