Chemical composition
Al Aluminum Rest Fe Iron 0.25 — 0.45 Si Silicon 0.15 — 0.35 Mg Magnesium <0.05 Mn Manganese 1.0 — 1.4 Cu Copper <0.1 Ti Titanium <0.1 Zn Zinc <0.1 OE Other items <0.05 ET Total other items <0.1
Analogs in Germany
AG1
AG15
AlMnCu DIN 1725 Part 1
3.0517 DIN 1725 Part 1
AlMn1 DIN 1725 Part 1
3.0515 DIN 1725 Part 1
EN AW-3003 DIN EN 12392: 2016
EN AW-AlMn1Cu DIN EN 12392: 2016
EN AW-3103 DIN EN 12392: 2016
EN AW-AlMn1 DIN EN 12392: 2016
EN AW-3003 DIN EN 12392: 2016 / A1: 2019
EN AW-AlMn1Cu DIN EN 12392: 2016 / A1: 2019
EN AW-3103 DIN EN 12392: 2016 / A1: 2019
EN AW-AlMn1 DIN EN 12392: 2016 / A1: 2019
AW-3003 DIN EN 1301−2: 1997
AW-3103 DIN EN 1301−2: 1997
EN AW-3003 DIN EN 1301−2: 1997
AlMn1Cu DIN EN 1301−2: 1997
EN AW-3103 DIN EN 1301−2: 1997
AlMn1 DIN EN 1301−2: 1997
EN AW-3003 DIN EN 573−3: 2013
EN AW-AlMn1Cu DIN EN 573−3: 2013
EN AW-3103 DIN EN 573−3: 2013
EN AW-AlMn1 DIN EN 573−3: 2013
Analogs in Russia
3000
AMC Included in 7 Standards
AMTSM GOST 21631−76
AMTSN GOST 21631−76
AMtsN2 GOST 21631−76
AMTSSM GOST 21631−76
AMTSN GOST 21631−76
AMTSN2 GOST 21631−76
D9 GOST 2171−90
D10 GOST 2171−90
1400 GOST 4784−97
1401 GOST 4784−97
AMTSH GOST 4784−97
1400Sh GOST 4784−97
AMTSSSh GOST 4784−97
1401Sh GOST 4784−97
3003 GOST 745−14
AMTS GOST 9498−79
AMts OST 1 92014−90
1400 OST 1 92014−90
Analogs in the USA
AA3003 AA
4006 AMS
4008 AMS
4065 AMS
4067 AMS
AMS-A-22771 AMS
AMS-A-81596 AMS
AMS-QQ-A-200/1 AMS
AMS-QQ-A-225/2 AMS
AMS-QQ-A-250/2 AMS
AMS-QQ-A-250/3 AMS
AA3010 ANSI
AA3011 ANSI
AA3303 ANSI
AA3307 ANSI
AA3107 ANSI
AA3009 ANSI
AA3103 ANSI
3003 ANSI
SB 209 (3003) ASME SB209
SB 210 (3003) ASME SB210
SB 221 (3003) ASME SB221
SB 234 (3003) ASME SB234
SB 241 (3003) ASME SB241
SF A5.3 (E3003) ASME SF-A5.3
B 209 (3003) ASTM B209
B 210 (3003) ASTM B210
B 211 (3003) ASTM B211
B 221 (3003) ASTM B221
B 234 (3003) ASTM B234
B 241 (3003) ASTM B241
B 247 (3003) ASTM B247
B 275 (3003) ASTM B275
B 313 (3003) ASTM B313
B 316 (3003) ASTM B316
B 345 (3003) ASTM B345
B 404 Alloy 3003 ASTM B404
B 483 (3003) ASTM B483
B 491 (3003) ASTM B491
B 547 Alloy 3003 ASTM B547
B 548 (3003) ASTM B548
B 632 (3003) ASTM B632
B 736 (3003) ASTM B736
B 744 (3003) ASTM B744
B 745 (3003) ASTM B745
A5.3 (E3003) AWS A5.3
J454 (3003) SAE J454
A93003 UNS
For the manufacture of semi-finished products by hot or cold deformation. Technical requirements GOST 18482−18 Extruded pipes from aluminum and aluminum alloys. Specifications GOST 21631−76 Sheets from aluminum and aluminum alloys. Technical conditions GOST 4784−97 Aluminum and wrought aluminum alloys. Stamps
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 4784-97 | 0.25–0.45 | 0.15–0.35 | < 0.05 | 1–1.4 | < 0.1 | < 0.1 | < 0.1 | 97.35–98.6 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 2730 |
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|
| Trumpet | 100 | 12 | |||||
| Trumpet | annealing | 90–135 | 15 | ||||
| Trumpet | cold-work | 135 | |||||
| Round | GOST 21488-97 | 100 | 20 | ||||
| Tape | 100 | 10 | |||||
| Profile | 98 | 16 | |||||
| Sheet | 110–120 | 12–15 |
Analogues
| Germany | USA |
|---|---|
| 3003 | 3003 |
Standards
| Standard | Description |
|---|---|
| GOST 4784-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |