Amfu
Chemical composition
| Bi | Bismuth | <0.001 |
| Fe | Iron | <0.003 |
| Cu | Copper | Rest |
| As | Arsenic | <0.001 |
| Ni | Nickel | <0.002 |
| Sn | Tin | <0.002 |
| Pb | Lead | <0.002 |
| S | Sulfur | <0.003 |
| Ag | Silver | <0.003 |
| Sb | Antimony | <0.002 |
| P | Phosphorus | 0.03 — 0.08 |
| Zn | Zinc | <0.004 |
| Ot | Total impurities | <0.1 |
Cu-OFE DIN 1708
OF-Cu DIN 1708
SW-Cu DIN 1708
2.0061 DIN 1708
E1-Cu58 DIN 1708
E2-Cu58 DIN 1708
2.0062 DIN 1708
2.0040 DIN 1708
SE-Cu DIN 1708
2.0070 DIN 1708
2.0076 DIN 1708
SF-Cu DIN 1708
2.0090 DIN 1708
E-Cu57 DIN 1708
2.0060 DIN 1708
SW-Cu DIN 17670 Part 1
2.0076 DIN 17670 Part 1
E-Cu58 DIN 1787
2.0065 DIN 1787
OF-Cu DIN 1787
SW-Cu DIN 1787
2.0040 DIN 1787
2.0076 DIN 1787
Cu-OF DIN 40500 Part 5
2.0040 DIN 40500 Part 5
CU 101 DIN EN 1044: 1999
B-Cu100−1085 DIN EN 1044: 1999
Cu-DHP DIN EN 1057: 2006
CW024A DIN EN 1057: 2006
Cu-DHP DIN EN 12165: 2011
CW024A DIN EN 12165: 2011
Cu-OF DIN EN 12165: 2011
CW008A DIN EN 12165: 2011
Cu-ETP DIN EN 12165: 2011
CW004A DIN EN 12165: 2011
Cu-ETP DIN EN 12165: 2016
CW004A DIN EN 12165: 2016
Cu-OF DIN EN 12165: 2016
CW008A DIN EN 12165: 2016
Cu-DLP DIN EN 12167: 1998
CW023A DIN EN 12167: 1998
Cu-ETP DIN EN 12420: 2014
CW004A DIN EN 12420: 2014
Cu-OF DIN EN 12420: 2014
CW008A DIN EN 12420: 2014
Cu-DHP DIN EN 12449: 2012
CW024A DIN EN 12449: 2012
Cu-ETP DIN EN 12449: 2012
CW004A DIN EN 12449: 2012
Cu-ETP DIN EN 12449: 2016
CW004A DIN EN 12449: 2016
Cu-DHP DIN EN 12450: 2012
CW024A DIN EN 12450: 2012
Cu-DHP DIN EN 12451: 2012
CW024A DIN EN 12451: 2012
Cu-DHP DIN EN 12452: 2012
CW024A DIN EN 12452: 2012
Cu-DHP DIN EN 12735−1: 2010
CW024A DIN EN 12735−1: 2010
Cu-DHP DIN EN 12735−2: 2010
CW024A DIN EN 12735−2: 2010
Cu-ETP DIN EN 13148: 2010
CW004A DIN EN 13148: 2010
Cu-OF DIN EN 13148: 2010
CW008A DIN EN 13148: 2010
Cu-DHP DIN EN 13148: 2010
CW024A DIN EN 13148: 2010
Cu-ETP DIN EN 13347: 2003
CF004A DIN EN 13347: 2003
Cu-DHP DIN EN 13348: 2008
CW024A DIN EN 13348: 2008
Cu-DHP DIN EN 13349: 2002
CW024A DIN EN 13349: 2002
Cu-OF DIN EN 13599: 2014
CW008A DIN EN 13599: 2014
Cu-ETP DIN EN 13599: 2014
CF004A DIN EN 13599: 2014
Cu-ETP DIN EN 13600: 2013
CF004A DIN EN 13600: 2013
Cu-OF DIN EN 13600: 2013
CW008A DIN EN 13600: 2013
Cu-OFE DIN EN 13600: 2013
CW009A DIN EN 13600: 2013
Cu-ETP DIN EN 13601: 2013
CW004A DIN EN 13601: 2013
Cu-FRHC DIN EN 13601: 2013
CW005A DIN EN 13601: 2013
Cu-OF DIN EN 13601: 2013
CW008A DIN EN 13601: 2013
Cu-ETP DIN EN 13602: 2013
CW004A DIN EN 13602: 2013
Cu-OF DIN EN 13602: 2013
CW008A DIN EN 13602: 2013
Cu-OFE DIN EN 13604: 2013
CW009A DIN EN 13604: 2013
Cu-ETP DIN EN 13605: 2013
CW004A DIN EN 13605: 2013
Cu-OF DIN EN 13605: 2013
CW008A DIN EN 13605: 2013
Cu-DHP DIN EN 14436: 2004
CW024A DIN EN 14436: 2004
Cu-ETP DIN EN 14436: 2004
CF004A DIN EN 14436: 2004
Cu-OF DIN EN 14436: 2004
CW008A DIN EN 14436: 2004
Cu-ETP DIN EN 1652: 1998
CW004A DIN EN 1652: 1998
Cu-OF DIN EN 1652: 1998
CW008A DIN EN 1652: 1998
Cu-DLP DIN EN 1652: 1998
CW023A DIN EN 1652: 1998
Cu-DLP DIN EN 1653: 1998
CW023A DIN EN 1653: 1998
Cu-FRHC DIN EN 1976: 2012
CR005A DIN EN 1976: 2012
Cu-OF DIN EN 1976: 2012
CR008A DIN EN 1976: 2012
Cu-DLP DIN EN 1976: 2012
CR023A DIN EN 1976: 2012
Cu-DHP DIN EN 1976: 2012
CR024A DIN EN 1976: 2012
Cu-ETP DIN EN 1976: 2012
CR004A DIN EN 1976: 2012
Cu-ETP DIN EN 1977: 2013
CW004A DIN EN 1977: 2013
Cu-OF DIN EN 1977: 2013
CW008A DIN EN 1977: 2013
Cu-OFE DIN EN 1977: 2013
CW009A DIN EN 1977: 2013
Cu-OFE DIN EN 2085: 2007
CW009A DIN EN 2085: 2007
CU1 DIN EN 28839
CU-BU9001 DIN EN 3963: 2001
CU-BU9001 DIN EN 3964: 2001
Cu-ETP DIN EN 50149: 2012
CW004A DIN EN 50149: 2012
Cu-OFE DIN EN CEN / TS 13388
CR009A DIN EN CEN / TS 13388
CW009A DIN EN CEN / TS 13388
Cu-OFE DIN EN CEN / TS 13388
CR009A DIN EN CEN / TS 13388
CW009A DIN EN CEN / TS 13388
Cu-ETP DIN EN CEN / TS 13388
CR004A DIN EN CEN / TS 13388
CW004A DIN EN CEN / TS 13388
Cu-OF DIN EN CEN / TS 13388
CR008A DIN EN CEN / TS 13388
CW008A DIN EN CEN / TS 13388
Cu-ETP DIN EN CEN / TS 13388
CF004A DIN EN CEN / TS 13388
Cu-OF DIN EN CEN / TS 13388
CF008A DIN EN CEN / TS 13388
B-Cu100−1085 DIN EN CEN / TS 13388
CF032A DIN EN CEN / TS 13388
CU 101 DIN EN CEN / TS 13388
Cu 102 DIN EN ISO 17672
Cu 110 DIN EN ISO 17672
KME 100 KME
COPPER Cu a 1 ThyssenKrupp
SE-Cu Included in 2 standards
SF-Cu Included in 2 standards
2.0090 Included in 2 standards
2.0070 Included in 2 standards
E-Cu Included in 2 Standards
2.0060 Included in 5 standards
E-Cu57 Included in 7 Standards
Analogs in Russia
M1 Included in 2 Standards
M001b Included in 2 standards
M1E Included in 2 Standards
M00b Included in 3 standards
M0b Included in 3 standards
M1b Included in 3 standards
M1 Included in 6 Standards
M1 Included in 8 Standards
M0b GOST 10988−16
M0b GOST 10988−75
M1 GOST 1173−06
M1E GOST 1173−06
M0b GOST 15040−16
M1 GOST 1535−06
M1E GOST 1535−06
M0b GOST 4752−12
M1 GOST 617−06
AMF GOST 767−91
M1u GOST 767−91
M0k GOST 859−01
M00b GOST 859−01
M0b GOST 859−01
M0 GOST 859−01
M1b GOST 859−01
M1E GOST 859−01
M0k GOST 859−14
M0 GOST 859−14
M0b GOST R 53405−09
M001 GOST R 53803−10
M0 GOST R 53803−10
M0b GOST R 53803−10
M1or GOST R 53803−10
MCH0 GOST R 54310−11
CU1 GOST R ISO 8839
MF TU 48−21−5045−80
M1 TU 48−21−529−82
MCH0 TU 48−7-21−89
Analogs in the USA
BCu-1b
Cu 100
ETP
OF
OF
OF
ETP
C 11000 AMS4500H
4501D AMS4501D
4602C AMS4602C
SB 111 (C10200) ASME SB111
SB 111 (OF) ASME SB111
SB 152 (C10200) ASME SB152
SB 152 (C11000) ASME SB152
SB 152 (OF) ASME SB152
SB 152 (ETP) ASME SB152
SB 152 (TP) ASME SB152
SB 187 (C10200) ASME SB187
SB 187 (C11000) ASME SB187
SB 188 (C10200) ASME SB188
SB 188 (OF) ASME SB188
SB 188 (C11000) ASME SB188
SB 188 (ETP) ASME SB188
SB 283 (C11000) ASME SB283
SB 359 (C10200) ASME SB359
SB 395 (C10200) ASME SB395
SB 395 (OF) ASME SB395
B 395 (C10200) ASME SB395
B 395 (OF) ASME SB395
SB 42 (C10200) ASME SB42
SB 42 (OF) ASME SB42
SB 75 (C10200) ASME SB75
SF A5.8 (BCu-1b) ASME SF-A5.8
SF 467 (110) ASME SF467
SF 467 (C11000) ASME SF467
SF 467 (Cu 110) ASME SF467
F 467MA ASME SF467
SF 468 (110) ASME SF468
SF 468 (C11000) ASME SF468
SF 468 (Cu 110) ASME SF468
F 468MA ASME SF468
B 1001 Type ETP ASTM B1001
B 1001 (C11000) ASTM B1001
B 111 (C10200) ASTM B111
B 111 (OF) ASTM B111
B 116 (C10100) ASTM B116
B 116 (C10200) ASTM B116
B 116 (C11000) ASTM B116
B 116 (C11040) ASTM B116
B 124 (C11000) ASTM B124
B 133 (C 11000) ASTM B133
B 152 (C10200) ASTM B152
B 152 (C11000) ASTM B152
B 152 (OF) ASTM B152
B 152 (ETP) ASTM B152
B 152 (TP) ASTM B152
B 170 Grade 2 ASTM B170
B 170 (C10200) ASTM B170
B 187 (C10200) ASTM B187
B 187 (C11000) ASTM B187
B 188 (C10200) ASTM B188
B 188 (OF) ASTM B188
B 188 (C11000) ASTM B188
B 188 (ETP) ASTM B188
B 272 (C10200) ASTM B272
B 272 (C11000) ASTM B272
B 280 (C10200) ASTM B280
B 280 (OF) ASTM B280
B 283 (C11000) ASTM B283
B 359 (C10200) ASTM B359
B 372 (C10200) ASTM B372
Copper, Type OF ASTM B372
B 395 (C10200) ASTM B395
B 395 (OF) ASTM B395
B 42 (C10200) ASTM B42
B 42 (OF) ASTM B42
B 447 (C10200) ASTM B447
B 447 (C11000) ASTM B447
B 451 (99.95 Cu-.040) ASTM B451
B 49 (C11000) ASTM B49
B 49 Type ETP ASTM B49
B 49 (C11040) ASTM B49
B 49 Type ETP ASTM B49
B 49 (C10100) ASTM B49
B 49 Type OFE ASTM B49
B 49 (C10200) ASTM B49
B 49 Type OF ASTM B49
B 5 (C11000) ASTM B5
B 5 (ETP) ASTM B5
B 638 (C 11000) ASTM B638
B 640 (C 10200) ASTM B640
B 640 (C10200) ASTM B640
B 68 (C10200) ASTM B68
B 698 (C10200) ASTM B698
B 698 (OF) ASTM B698
B 738 (C10100) ASTM B738
B 738 (C10200) ASTM B738
B 738 (C11000) ASTM B738
B 738 (C11040) ASTM B738
B 738 Type ETP ASTM B738
B 738 Type ETP ASTM B738
B 738 Type OF ASTM B738
B 738 Type OFE ASTM B738
B 743 (C10200) ASTM B743
B 75 (C10200) ASTM B75
B 88 (C10200) ASTM B88
B 919 (C10200) ASTM B919
F 467 (C11000) ASTM F467
F 467 (110) ASTM F467
F 467 (Cu 110) ASTM F467
F 467MA ASTM F467
F 468 (C11000) ASTM F468
F 468 (110) ASTM F468
F 468 (Cu 110) ASTM F468
F 468MA ASTM F468
A5.8 (BCu-1b) AWS A5.8
C 11000 CDA
ETP CDA
OF CDA
J463 (C 11000) SAE J463
C11000 UNS
C10200 UNS
99.95Cu-.040 Included in 11 standards
For the manufacture of hot-rolled and cold-rolled anodes used for galvanic coating of products. Technical requirements GOST 767−91 Copper anodes. Technical conditions
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | P, % | S, % | Ag, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 767-91 | < 0.003 | < 0.002 | < 0.001 | 99.903–99.97 | < 0.004 | < 0.002 | < 0.002 | < 0.002 | < 0.001 | 0.03–0.08 | < 0.003 | < 0.003 |
Information on suppliers
Analogues
| Germany |
|---|
| Cu-OFE DIN 1708 |
Standards
| Standard | Description |
|---|---|
| GOST 767-91 | GOST 767 - 91 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |
| Ag | % | Silver |