AMg1M1
For the production of flat ingots, designed for rolling sheets, tapes and other semi-finished products.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Ti, % | Cu, % | Zn, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| GOST 9498-79 | < 0.7 | < 0.7 | 0.8–1.3 | 1–1.5 | < 0.2 | < 0.25 | < 0.2 | 95.15–98.2 |