AMST
For obtaining bimetallic strip steel by rolling and subsequent punching of liners with a thickness of friction layer is less than 0.5 mm.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Antifriction aluminum alloy |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Ti, % | Cu, % | Zn, % | Sb, % | Al, % | Te, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 14113-78 | < 0.75 | < 0.5 | < 0.2 | 0.03–0.12 | 0.7–1.2 | < 0.1 | 4.6–6.5 | 90.03–94.64 | 0.03–0.3 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 14113-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Ti | % | Titan |
| Cu | % | Copper |
| Zn | % | Zinc |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Te | % | Tellurium |