Nickel alloy ANV-300
Chemical composition
Al Aluminum 4.5 — 5.5 B Boron <0.1 W Tungsten 7.0 — 10.0 Si Silicon <0.5 Mn Manganese <0.5 Mo Molybdenum <0.5 Ni Nickel Rest S Sulfur <0.01 Ti Titanium 1.4 — 2.0 C Carbon <0.1 P Phosphorus <0.015 Cr Chromium 14.0 — 17.0
Mo: as agreed
Analog in Russia — ANV-300 OST 1 90127−85
Production of ingots and cast rods intended for further remelting in the manufacture of shaped castings. Technical requirements OST 1 90127−85 Heat-resistant foundry alloys of open smelting OST 1 90127−85 Heat-resistant foundry alloys of open smelting
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant alloys |
Chemical composition
| Standard | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | Al, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| OST 1-90127 - 85 | < 0.5 | < 0.1 | < 0.5 | 14–17 | 1.4–2 | 63.775–73.1 | 4.5–5.5 | < 0.015 | < 0.1 | < 0.01 | < 0.5 | 7–10 |
Information on suppliers
Long-term strength
| Standard | Treatment | Температура испытаний, ° С | Постоянно приложенное напряжение, МПа | Время до разрушения в часах, ч |
|---|---|---|---|---|
| OST 1-90127 - 85 | Heating to a temperature of 1120 ± 10 ° С, holding 10 hours, air cooling | 850 | 250 | 60 |
Standards
| Standard | Description |
|---|---|
| OST 1-90127 - 85 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |