Alloy aluminum AO12-1
- Chemical composition
| Al | Aluminum | Rest |
| Fe | Iron | <0.3 |
| Cu | Copper | 0.8 — 1.2 |
| Ni | Nickel | 0.4 — 0.6 |
| Sn | Tin | 11.0 — 14.0 |
| OE | Other items | <0.05 |
| ET | Total other items | <0.55 |
| GOST 14113−78 | Alloys aluminum antifriction. Stamps. |
To obtain a bimetallic tape with steel by rolling. used for the manufacture of plain bearings of automotive and tractor equipment. Technical requirements for TU DAYDO METAL RUSS
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Antifriction aluminum alloy |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Ni, % | Al, % |
|---|---|---|---|---|---|
| GOST 14113-78 | < 0.3 | 11–14 | 0.8–1.2 | 0.4–0.6 | 84.5–87.8 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 14113-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Cu | % | Copper |
| Ni | % | Nickel |
| Al | % | Aluminium |