Alloy aluminum AO9-2
Chemical composition
| Al |
Aluminum |
Rest |
| Fe |
Iron |
<0.5 |
| Si |
Silicon |
0.3 — 0.7 |
| Cu |
Copper |
2.0 — 2.5 |
| Ni |
Nickel |
0.8 — 1.2 |
| Sn |
Tin |
8.0 — 10.0 |
| OE |
Other items |
<0.1 |
For casting monometallic liners and bushings Technical requirements — according to GOST 14113−78
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Antifriction aluminum alloy |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Cu, % |
Ni, % |
Al, % |
| GOST 14113-78 |
< 0.5 |
0.3–0.7 |
8–10 |
2–2.5 |
0.8–1.2 |
85.5–88.9 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
3000 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Casting |
|
|
|
in chill mold |
130–170 |
78–105 |
2.3–6.3 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Casting |
|
in chill mold |
500–600 |
Casting and technological parameters
| melting point, °C |
| 226–650 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |